In continuously reinforced concrete pavement, the area enclosed by two closely spaced (less than 3 ft or 1m) transverse cracks, a short longitudinal crack, and the edge of the pavement or longitudinal joint, when exhibiting spalling, shattering, or faulting. Also, area between Y cracks exhibiting this same deterioration.